1] Enlargement of Dead Man Zone
2] Poor hearth Annulus
3] prolonged operation in low blast
4] Insufficient cooling water pressure at tuyre
5] Coke value CRI CSR
6] Manufaturing Defect in tuyre.
7] Viscosity of the slag
8] High Pressure drop in furnace